[Clayart] Cone 6 clay
wschran at twc.com
wschran at twc.com
Thu Aug 23 13:24:17 EDT 2018
Think due to sulfur content.
William Schran
wschran at twc.com
703-505-1617
---- Rod Haaland <rod.haaland at gmail.com> wrote:
> Why no goldart?
On Wed, Aug 22, 2018 at 12:41 PM Douglas Fur <23drb50 at gmail.com> wrote:
> Based on my tests, I would build an orange clay body starting with these
> parameters.
>
> Hawthorne FC yes
> Lincoln FC no
> OM4 only if needed {bentonite might be a better choice}
> Goldart not so much
> Tri-calcium phosphate yes
> Ocher yes
> Rutile (I saw negligible effect in one series and didn't pursue it. It
> might enhance the color produced by ocher.)
> Gerstley borate (theoretically a clay with boron and phosphorus in the
> glassy matrix would be stronger.) Interesting but
> needs work. Can produce a "cakey" texture but this can
> be offset by adding vinegar.
>
> If I were starting this morning my guess would be
> 80 Hawthorne
> 10 grog
> 7 TCP
> 3 ocher
>
> Duff
> Seola Creek
> -------------- next part --------------
> An HTML attachment was scrubbed...
> URL: <
> https://lists.clayartworld.com/pipermail/clayart/attachments/20180822/1218b966/attachment.html
> >
>
--
Rod Haaland
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <https://lists.clayartworld.com/pipermail/clayart/attachments/20180823/278c8506/attachment.html>
More information about the Clayart
mailing list